Trademark  | Code  | Applications  | 
HT200  | C.I.  | Water below 80 ℃  | 
GCr15  | GCr15  | Bearing steel  | 
QT500  | QT  | Water pump housing  | 
ZG230-450  | ZG25  | Water, oil  | 
42CrMo  | 4140  | Shaft  | 
1Cr13  | 410  | Food, oil  | 
2Cr13  | 420  | Shaft  | 
1Cr13Ni  | 410S  | High-pressure water pump housing, balance disc, etc.  | 
1Cr18Ni9  | 302  | Alkaline, acidic water  | 
0Cr18Ni9  | 304  | Alkaline, acidic water  | 
1Cr18Ni12  | 305  | Acidic water  | 
0Cr25Ni20  | 310S  | Caustic soda  | 
1Cr18Ni12Mo2Ti  | M  | Dilute sulfuric acid, phosphoric acid, organic acids  | 
00Cr17Ni14Mo2  | 316L  | Dilute nitric acid, phosphoric acid, organic acid  | 
00Cr19Ni13Mo3  | 317L  | Ibid, resistance to intergranular corrosion  | 
1Cr18Ni9Ti  | 321  | Alkaline, acidic water, organic acids  | 
00Cr20Ni25Mo4.5Cu  | 904L  | Various concentrations of sulfuricacid below 70 ℃  | 
0Cr30Ni42Mo3Cu2  | 804  | Caustic soda 150 ℃  | 
0Cr20Ni42Mo3Cu2  | 824  | 904 is still impatient corrosion  | 
0Cr21Ni32Mo2Cu3  | 20 # alloy  | Hot concentrated sulfuric acid, T ≤ 130 ℃, 40% concentration  | 
0Cu24Ni20Mo2Cu3  | K alloy  | ≤ 60% of various concentrations of sulfuric acid  | 
00Cr10Ni20Si6Mo  | 920  | Hot concentrated sulfuric acid, T ≤ 130 ℃, the concentration of 93-98%  | 
00Cr25Ni6Mo2  | MM-4  | Special steel nitrophosphate  | 
0Cr17Ni7Al  | 631  | The long axis of liquid pumps  | 
N6  | Pure Nickel  | High temperature caustic soda, alkali evaporator  | 
0Ni60Mo22Fe20  | Hastelloy A  | Various concentrations of hydrochloric acid below 70 ℃  | 
00Ni65Mo28  | Hastelloy B  | All concentrations of hydrochloric acid  | 
0Ni60Mo18Fe8Cr17Cu3Mn  | Hastelloy C  | Cold nitric acid, hypochlorous acid,hydrofluoric acid, etc.  | 
00Cr30Ni40Mo4Cu3  | Lewmet55  | All full-temperature sulfuric acid concentration  | 
00Ni65Cu28  | Monel  | Hydrofluoric acid, silicon fluoride acid, high temperature caustic soda  | 
00Cr14Ni14Si4  | C4  | Full concentration of nitrate  | 
TiAl6V4  | TC4  | Oxidizing corrosive media  | 
TA2  | Ti  | Mother liquor of soda ash, sea water  | 
0Cr26Ni5Mo2Cu3  | CD4MCu  | Solid containing dilute sulfuric acid, phosphoric acid, wear and corrosion  | 
F30%CrMo  | Cr30  | Phosphoric acid slurry, more wear and corrosion  | 
00Cr25Ni6Mo2  | MM-4  | Nitrate, phosphate-specific  | 
0Cr27Ni31Mo4.5Cu2  | ZS28  | Hydrochloric acid slurry  | 
STSi15  | G  | Nitric acid, chromic acid, sulfuric acid, etc. (excluding HCl)  | 
Cr28  | E  | Concentrated nitric acid  | 
Cr30  | F30%CrMo  | For corrosive and abrasive media  | 
0Cr18Ni5Mo5  | NH55  | Seawater  | 
00Cr22Ni5Mo3N  | SAF2205  | Seawater  | 
00Cr25Ni7Mo4N  | SAF2507  | Water, better than SAF2205  | 
0Cr17Ni17Si5  | 05  | High concentration, high temperature sulfuric acid  | 
1Cr26Ni6  | PH50  | Casing wear ring  | 
STNiCr202  | Nickel-iron  | High temperature and high concentration of caustic soda  | 
| TiMo32 | 32 Mo Titanium Alloy  | Oxidation and reduction of corrosive media  | 
TiMo0.3Ni0.8  | Ti, Mo, Ni alloys  | Oxidative corrosion medium, crevice corrosion resistance  | 
TiTa5  | Titanium tantalum alloys  | Hot concentrated nitric acid and synthetic resins and other strong corrosive media  |